MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ferro Aluminum Oxide P96
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Manufactured at the Diamonite Plant in Shreve, Ohio. Data provided by the manufacturer, Ferro Corporation.

Key Words: Al2O3, alumina, aluminium oxide, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.75 g/cc0.135 lb/in³
Water Absorption 0.00 %0.00 %
Open Porosity 0.00 %0.00 %Gas tight. Test with helium mass spectrometer
Weibull Modulus 1212
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 11851185KHN5 microhardness, kg/mm²
Vickers Microhardness 12551255HV5 microhardness, kg/mm²
Tensile Strength, Ultimate 151 MPa21900 psiACMA Test #4
Modulus of Elasticity 310 GPa45000 ksiultrasonic
Compressive Strength 2241 MPa325000 psiASTM C773-74
Poissons Ratio 0.250.25ASTM C623
Fracture Toughness 3.70 MPa-m½3.37 ksi-in½Kic (indentation)
Shear Modulus 124 GPa18000 ksiultrasonic
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  3.50e+6 ohm-cm
@Temperature 700 °C
3.50e+6 ohm-cm
@Temperature 1290 °F
ASTM D257
 5.80e+7 ohm-cm
@Temperature 500 °C
5.80e+7 ohm-cm
@Temperature 932 °F
ASTM D257
 1.40e+10 ohm-cm
@Temperature 300 °C
1.40e+10 ohm-cm
@Temperature 572 °F
ASTM D257
 1.80e+14 ohm-cm
@Temperature 100 °C
1.80e+14 ohm-cm
@Temperature 212 °F
ASTM D257
Dielectric Constant 9.5
@Frequency 1e+6 Hz
9.5
@Frequency 1e+6 Hz
ASTM D-116
Dielectric Strength 8.15 kV/mm
@Thickness 6.35 mm
207 kV/in
@Thickness 0.250 in
ASTM D149
Dissipation Factor 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
ASTM D-116
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.40 µm/m-°C
@Temperature 25.0 - 200 °C
3.00 µin/in-°F
@Temperature 77.0 - 392 °F
ASTM C32
 7.40 µm/m-°C
@Temperature 25.0 - 500 °C
4.11 µin/in-°F
@Temperature 77.0 - 932 °F
ASTM C32
 8.10 µm/m-°C
@Temperature 25.0 - 800 °C
4.50 µin/in-°F
@Temperature 77.0 - 1470 °F
 8.50 µm/m-°C
@Temperature 25.0 - 1000 °C
4.72 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM C32
Thermal Conductivity 28.5 W/m-K198 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 96 %96 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Ferro Aluminum Oxide P3142
AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1045 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round

CFC011 / 809

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.