MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Goodfellow C-Solder for Carbon Material Joining
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Material Notes: C-Solder is the trade name for a group of new tin-based, lead-free low-temperature soldering alloys which enable the joining of various carbon materials, including carbon fibers or carbon nanotube fibers, in both carbon-carbon and carbon-metal combinations. The resultant bond is mechanically strong and electrically conductive.

Characteristics:

  • Excellent flow
  • Good wetting of surfaces to be joined
  • Aluminum to Aluminum can be soldered without using flux.
  • Carbon can be soldered to metals (e.g. Copper, Aluminum), Ceramics and Glass materials
  • Not affected by cleaning solvents
  • Does not leave residues
  • Not flammable
  • Flux Free
  • Lead Free
  • RoHS Compliant

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.40 g/cc0.267 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 232 °C>= 450 °FSolidus
Solidus 232 °C450 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 - 450 °C455 - 842 °FSoldering temp
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 2 - 6 %2 - 6 %
Copper, Cu 0.01 - 1 %0.01 - 1 %
Silver, Ag 3 - 5 %3 - 5 %
Tin, Sn 90 - 100 %90 - 100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eifeler Coatings Technology TiN/TiC CVD Coating
Eifeler Coatings Technology TiN PVD Coating
Eifeler Coatings Technology TiC/TiN CVD Coating
Johnson Matthey JM 99C Soft Solder/Flux
Johnson Matthey JM 97C Soft Solder/Flux

NGOODF090 / 239183

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.