MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poco Graphite HPD Semiconductor Grade Graphite
Categories: Carbon; Graphite

Material Notes: Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their performance under specific conditions. The manufacturing process for each grade is tightly controlled to produce materials that have a uniform microstructure and the right balance of strength, grain size and hardness to offer optimum performance for their intended applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 1.77 g/cc0.0639 lb/in³
Particle Size 5.0 µm5.0 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength, Yield 60.0 MPa8700 psiEstimated at 70% of flexural strength
Flexural Strength 90.0 MPa13100 psi
Compressive Strength 150 MPa21800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00200 ohm-cm0.00200 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.10 µm/m-°C4.50 µin/in-°F
Thermal Conductivity 85.0 W/m-K590 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Poco Graphite ZXF-5Q Industrial Grade Graphite
Poco Graphite AXZ-5Q Industrial Grade Graphite
Poco Graphite CZR Semiconductor Grade Graphite
Poco Graphite PLS Semiconductor Grade Graphite
Poco Graphite SFG Semiconductor Grade Graphite

CPOCO17 / 85594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.