MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daicel CEVIAN® A1700 PA/ABS Alloy, DAM
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Property data is for dry as molded (DAM) samples.

Information provided by PlastxWorld Inc.

Key Words: Polyamide + Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D792
Water Absorption 0.98 %0.98 %24 hr; ASTM D570
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 116116ASTM D785
Tensile Strength, Yield 46.9 MPa6800 psiASTM 638
Elongation at Break 100 %100 %ASTM D635
Flexural Yield Strength 75.2 MPa10900 psiASTM D790
Flexural Modulus 2.16 GPa313 ksiASTM D790
Izod Impact, Notched 1.55 J/cm
@Thickness 3.17 mm
2.90 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C221 °F0.25 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °F0.25 inch; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Plastiblend® ABS/PA 1700
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy
Americhem Engineered Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Daicel CEVIAN® A1700 PA/ABS Alloy, Conditioned
Polykemi AB SCANLON A 5005B PA/ABS-Blend

PPLASTX04 / 56408

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.