MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastics Group Polifil® GFPC-20 20% Glass-Reinforced Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycarbonate line an excellent choice for electrical, appliance and hardware applications. Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Density 1.35 g/cc0.0488 lb/in³ASTM D792
Filler Content 20 %20 %ASTM D2584
 20.0 %20.0 %TPG WI
Water Absorption 0.200 %
@Time 86400 sec
0.200 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage  0.0020 - 0.0030 cm/cm
@Thickness 1.59 mm
0.0020 - 0.0030 in/in
@Thickness 0.0625 in
ASTM D955
 0.00300 cm/cm
@Thickness 3.17 mm
0.00300 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 12 - 20 g/10 min12 - 20 g/10 min300/1.2; May be specified; ASTM D1238
 7.00 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.00 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9393ASTM D785
Hardness, Rockwell R 120120ASTM D785
Tensile Strength at Break 109 MPa15800 psiASTM D638
Tensile Strength 109 MPa15800 psiASTM D638
Elongation at Break 5.00 %5.00 %ASTM D638
 6.0 %6.0 %ASTM D638
Elongation at Yield 3.00 %3.00 %ASTM D638
Tensile Modulus 5.864 GPa850.5 ksiASTM D790
 5.87 GPa851 ksiASTM D638
Flexural Strength 131 MPa19000 psiASTM D790
 131 MPa19000 psiASTM D790
Flexural Modulus 5.38 GPa780 ksiTangent; ASTM D790
 5.38 GPa780 ksitangent; ASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inAt 73°F; ASTM D256
 1.33 J/cm2.50 ft-lb/inASTM D256
Gardner Impact 0.452 J
@Thickness 12.7 mm
0.333 ft-lb
@Thickness 0.500 in
tup; ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FASTM D648
 146 °C295 °FASTM D648
Flammability, UL94 HBHB
 HBHB
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 221 °C410 - 430 °F
Middle Barrel Temperature 216 - 227 °C420 - 440 °F
Front Barrel Temperature 227 - 238 °C440 - 460 °F
Nozzle Temperature 227 - 249 °C440 - 480 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastics Group Polifil® GFRMPPCC-20 20% Glass Reinforced Polypropylene, High Impact
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene
Plastics Group Polifil® GFPP-20 20% Glass-Reinforced Polypropylene
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 20 wt.% glass

PPOLI039 / 56943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.