MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® AKV 25 FN00 000000 Nylon 66 (PA66), 25% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: PA 66, 25% glass fibers, injection molding, halogen free flame retardant

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³ISO 60
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.5 %1.5 %50% RH; ISO 62
Water Absorption at Saturation 4.6 %4.6 %ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/in60x60x2; 270 °C / WZ 120°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in60x60x2; 270 °C / WZ 120°C; 600 bar; ISO 294-4
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 270 °C
12 g/10 min
@Load 4.76 lb,
Temperature 518 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psi5 mm/min; ISO 527-1,-2
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527-1,-2
 3.4 %3.4 %50 mm/min, Nominal; ISO 527-1,-2
Tensile Modulus 9.60 GPa1390 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 210 MPa30500 psi2 mm/min; ISO 178-A
Flexural Modulus 9.10 GPa1320 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 3.3 %3.3 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched <= 1.00 J/cm²
@Temperature 23.0 °C
<= 4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.40e+13 ohm-cm7.40e+13 ohm-cmIEC 60093
Surface Resistance 1.10e+16 ohm1.10e+16 ohmIEC 60167
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
Comparative Tracking Index 0.00 V0.00 VSolution A; UL 746A
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air 228 °C442 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FISO 75-1,-2
Vicat Softening Point 225 °C
@Load 5.10 kg
437 °F
@Load 11.2 lb
120°C/h; ISO 306
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
Oxygen Index 38 %38 %Method A; ISO 4589-2
Glow Wire Ignition Temperature  775 °C
@Thickness 0.400 mm
1430 °F
@Thickness 0.0157 in
IEC 60695-2-13
 775 °C
@Thickness 0.750 mm
1430 °F
@Thickness 0.0295 in
IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
1430 °F
@Thickness 0.0591 in
IEC 60695-2-13
 775 °C
@Thickness 3.00 mm
1430 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
IEC 60695-2-12
 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
Shrinkage, MD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.10 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Flow Direction Post-Molding, 60x60x2; ISO 294-4
Shrinkage, TD 0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.10 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Molding, 60x60x2; ISO 294-4
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °Finjection molding; ISO 294
 265 - 285 °C509 - 545 °F
Mold Temperature 80.0 °C176 °Finjection molding; ISO 294
 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 6.00 hour2.00 - 6.00 hour
Moisture Content 0.030 - 0.070 %0.030 - 0.070 %Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 25 FN01 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Dry)
Envalior Durethan® AKV 25 F30 000000 Nylon 66 (PA66), 25% Glass Fiber Reinforced, Dry
Overview of materials for Nylon 66, 30% Glass Fiber Filled

PLANW9210 / 208007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.