MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® D1101 (SBS) Linear Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact qualities of the material, both at room and low temperature. This KRATON polymer meets FDA regulations as articles or as ingredients in articles intended for food contact. FDA clearances vary from one grade to another. For specific clearances, letters of certification will be provided on request.

Applications: modified asphalts, thermoplastic and thermoset polymer modification, adhesives, sealants, coatings, sporting goods, film, and general elastomer compounding.

Information provided by the manufacturer, Kraton® Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/cc
Brookfield Viscosity 4000 cP
@Temperature 25.0 °C
4000 cP
@Temperature 77.0 °F
Toluene solution. Neat polymer concentration, 25%w.
Melt Flow <= 1.0 g/10 min<= 1.0 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 696910 seconds. Typical values on polymer compression molded at 150°C (300°F).
Tensile Strength, Ultimate 31.72 MPa4601 psiTensile tester jaw separation 10 in/min (25.4 cm/min). Typical properties based on film cast from toluene solution.; ASTM D412
Elongation at Break 880 %880 %Tensile tester jaw separation 10 in/min (25.4 cm/min); ASTM D412
300% Modulus 2.76 MPa
@Strain 300 %
400 psi
@Strain 300 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm1.00e+14 - 1.00e+16 ohm-cm
Dielectric Strength 11.81 - 39.37 kV/mm300.0 - 1000 kV/in
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -80.0 °C-112 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 200 °C302 - 392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D1102 (SBS) Linear Block Copolymer
Avient Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Kraton® D1116 (SB)n Branched Copolymer
Kraton® D4141 (SBS) Linear Block Copolymer

PKRA0010 / 49061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.