MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

E-Polymers EFLEX® M200 Ethylene Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nylon and EVOH, as well as metal, polyolefins, cellulose, polyester, polycarbonate, glass, and foil. They are ideal for use as adhesives and tie layers in traditional food packaging applications and pipe coatings, and also in thermoplastic powder coatings, impact modification, modulus control, and glass-filled composites.

Information Provided by E-Polymers Co., Ltd.

Key Words: EPM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.870 g/cc0.870 g/ccASTM D792
Melt Flow 8.0 - 12 g/10 min
@Load 2.16 kg,
Temperature 280 °C
8.0 - 12 g/10 min
@Load 4.76 lb,
Temperature 536 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 53.0 °C127 °FASTM D3418
 
Descriptive Properties
MAH Graft LevelHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ethylene Propylene Rubber (EPM, EPDM)
Seals Eastern 7189 Ethylene-Propylene Rubber
Seals Eastern 7045 Ethylene-Propylene Rubber
DuPont Fusabond® MF416D Ethylene Propylene Rubber
Precision Polymer Engineering E50D Ethylene Propylene Rubber

PEPOLZ117 / 103614

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.