MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Addolink® TR Schuppen PU Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Information: Addolink TR Schuppen is used at low ratios only (about 2 - 10%, calculated on the total addition of crosslinking agent). Addolink TR Schuppen is miscible with Addolink B and Addolink R at all ratios. The reaction between Addolink TR Schuppen and polyisocyanates leads to three-dimensional crosslinking of the hard segment material; this reduces the segregation of the hard and soft segments in the elastomer. This effect can be utilized to reduce the Shore hardness of soft elastomers. It also improves their resistance to swelling, but reduces their tear strength. In hard elastomers it reduces shrinkage phenomena and stress cracking.

Function: Crosslinking agent for polyurethane elastomers (hot- and cold-curing cast systems).

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.09 g/cc
@Temperature 60.0 °C
0.0394 lb/in³
@Temperature 140 °F
 1.12 g/cc
@Temperature 20.0 °C
0.0405 lb/in³
@Temperature 68.0 °F
Water Absorption 0.10 %0.10 %
Viscosity 230 cP230 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 58.5 °C>= 137 °FFreezing Point
Flash Point 184 °C363 °FDIN EN 22719
 
Descriptive Properties
Appearanceclear liquidabove 60°C
 colorless and crystallineRT
Hydroxyl value>1235 mg KOH/g
Specifications99 percentActive ingredient

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Addolink® TR PU Additive
BASF Elastollan® S 60 AWH TPUR
Covestro Baytec® MS-080 Polyurethane
Covestro Desmopan® 3055D Polyurethane
BASF Elastollan® 1185 A W TPUR

PLANY8214 / 208607

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.