MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Xmod™ PC75 High Crystalline Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Xmod PC75 is a HCPP intended for injection molding of automotive interior parts. Xmod PC75 is a very easy-flowing material combined with a good balance between impact strength and stiffness. The material gives a good surface quality.

Xmod PC75 has been designed for pillar trims, door panels and pockets, and central consoles.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
Melt Flow 96 g/10 min
@Load 5.00 kg,
Temperature 230 °C
96 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 66.0 MPa9570 psiH 385/30; ISO 2039
Tensile Strength, Yield 26.0 MPa3770 psiAt 50 mm/min; ISO 527-2
Elongation at Yield 6.0 %6.0 %At 50 mm/min; ISO 527-2
Tensile Modulus 1.50 GPa218 ksiAt 1 mm/min; ISO 527-2
Flexural Modulus 1.40 GPa203 ksiAt 2 mm/min; ISO 178
Charpy Impact Unnotched 6.70 J/cm²
@Temperature -20.0 °C
31.9 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 0.320 J/cm²
@Temperature -20.0 °C
1.52 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °FISO 75-2
Vicat Softening Point 75.0 °C167 °FB (50N); ISO 306
 150 °C302 °FA (10N); ISO 306
Shrinkage 1.6 %1.6 %Borealis Method
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 260 °C410 - 500 °FPolymer Mass Temp
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
 
Descriptive Properties
Emissions, ug C/g 37VDA 277
Fogging, mg0.9At 100°C/ 16 hours

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications
Overview of materials for Polypropylene with 30% Glass Fiber Filler
Akro-Plastic Akromid® A3 GF 40 1 L black (4671) PA 6.6+PP Dry, 40% Glass Filled, Heat Stabilized

PBOREA216 / 27523

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.