MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Maxxam® MH-418.G001 Polypropylene (PP), Calcium Carbonate Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Description/Features:

  • Calcium Carbonate Filled
  • UL 94 HB
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0410 lb/in³ASTM D792
Filler Content 30 %30 %Reinforcement Level
Linear Mold Shrinkage 0.0090 - 0.013 cm/cm0.0090 - 0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7575ASTM D785
Tensile Strength, Yield 20.0 MPa2900 psiType 1 - Rigids, 2 in/min; ASTM D638
Elongation at Break 578 %578 %Type 1 - Rigids, 2 in/min; ASTM D638
Flexural Strength 25.5 MPa3700 psiASTM D790
Flexural Modulus 1.62 GPa235 ksiASTM D790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
1.50 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Gardner Impact 20.7 J
@Temperature -23.3 °C
15.3 ft-lb
@Temperature -10.0 °F
0.125 in.; ASTM D3029
Impact 14.114.1(ft-lb/in) Instr. Impact Energy to Max. Load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C190 °FAnnealed, 0.125 in bars; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0590 in
All Colors
 
Descriptive Properties
Product FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam® MH-418.F001 Polypropylene (PP), Calcium Carbonate Filled
Avient Maxxam® DP-8973-2 Polypropylene (PP), Calcium Carbonate Filled
Avient Maxxam® 8435 Polypropylene (PP), Calcium Carbonate Filled
Avient Maxxam® GZ-215 S002-1000 Polypropylene (PP), Calcium Carbonate Filled
Avient Maxxam® TR-218.F001 Polypropylene (PP), Calcium Carbonate Filled

PH1PO2664 / 44667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.