MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTANAT® TMDI Diisocyanate
Categories: Polymer

Material Notes: VESTANAT TMDI is an aliphatic diisocyanate, methyl group branched. It represents a mixture of the 2,2,4- and 2,4,4-trimethyl-hexamethylene diisocyanate (about 1:1). It is a low viscosity, colorless liquid with a weak but specific odor. It is light and weather resistant.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 - 1.016 g/cc
@Temperature 20.0 °C
0.0365 - 0.03671 lb/in³
@Temperature 68.0 °F
DIN 51 757
Viscosity 5.0 - 8.0 cP
@Temperature 23.0 °C
5.0 - 8.0 cP
@Temperature 73.4 °F
DIN EN ISO 3219
Vapor Pressure 0.00000270 bar0.00203 torr
 
Thermal PropertiesMetricEnglishComments
Flash Point 148 °C298 °Fclosed cup; DIN 51 758
Ignition Temperature 440 °C824 °FDIN 51 794
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4611.461DIN 51 423, Part 2
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl <= 0.0010 %<= 0.0010 %
 
Descriptive Properties
Hazen Color Index, max10DIN ISO 6271
NCO content (% wt)39.7-40EN ISO 11 909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fulcrum Composites Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod
Evonik REWOTERIC® AM 2 C NM Foam booster
Fulcrum Composites Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip
Evonik VESTANAT® PP PU prepregs
Evonik VESTANAT® IPDI Polyisocyanate

PHUMB408 / 81410

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.