MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott F2 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 620364.360
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.60 g/cc0.130 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 1.01.0
Alkali Class, AR 2.32.3
Stain Resistance Class, FR 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 420420.1/20
Modulus of Elasticity 57.0 GPa8270 ksi
Poissons Ratio 0.220.22
Shear Modulus 23.0 GPa3340 ksicalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.20 µm/m-°C
@Temperature -30.0 - 70.0 °C
4.56 µin/in-°F
@Temperature -22.0 - 158 °F
 9.20 µm/m-°C
@Temperature 20.0 - 300 °C
5.11 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.557 J/g-°C0.133 BTU/lb-°F
Thermal Conductivity 0.780 W/m-K5.41 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 434 °C813 °F
Softening Point 594 °C1100 °FViscosity 107.6 dPa s
Annealing Point 430 °C806 °FViscosity 1013.0 dPa s
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.62004
@Wavelength 587.6 nm
1.62004
@Wavelength 587.6 nm
nd
 1.62408
@Wavelength 546.1 nm
1.62408
@Wavelength 546.1 nm
ne
Abbe Number 36.1136.11ve
 36.3736.37vd
Optical Dispersion 0.017050.01705nf - nc
 0.0172840.017284nf' - nc'
Transmission, Visible  98.5 %
@Thickness 10.0 mm,
Wavelength 380 nm
98.5 %
@Thickness 0.394 in,
Wavelength 380 nm
 99.5 %
@Thickness 10.0 mm,
Wavelength 405 nm
99.5 %
@Thickness 0.394 in,
Wavelength 405 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 460 nm
99.8 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.9 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.9 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.9 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  80.9 %
@Thickness 10.0 mm,
Wavelength 2500 nm
80.9 %
@Thickness 0.394 in,
Wavelength 2500 nm
 99.6 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.6 %
@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance  8.0 %
@Thickness 10.0 mm,
Wavelength 320 nm
8.0 %
@Thickness 0.394 in,
Wavelength 320 nm
 53.7 %
@Thickness 10.0 mm,
Wavelength 334 nm
53.7 %
@Thickness 0.394 in,
Wavelength 334 nm
 97.5 %
@Thickness 10.0 mm,
Wavelength 370 nm
97.5 %
@Thickness 0.394 in,
Wavelength 370 nm
 
Descriptive Properties
B0
Climatic Resistance Test CR1
HG2
K (10-6mm2/N)2.81
Phosphate Resistance PR1.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Pyro-Tape™ 682-TB2-1 Thermal Barrier Ceramic Tape
Aremco Pyro-Tape™ 682-TB1-2 Thermal Barrier Ceramic Tape
American Computer Optics 15in Tempered LCD Glass
3M Nextel™ BP-18 Woven Tape 312 (5.1 cm)
3M Nextel™ BP-18 Woven Tape 312 (3.8 cm)

CSGS046 / 93380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.