MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Global 100-25 LDPE Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Commercial-grade, low-density polyethylene with good dimensional stability, toughness and softness.
  • Good dimensional stability
  • Soft
  • Good toughness

Applications:

  • Caps
  • Closures

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50
@Thickness 3.17 mm
50
@Thickness 0.125 in
Durometer, Injection Molded; ASTM D2240
Tensile Strength at Break 56.5 MPa
@Thickness 3.17 mm
8200 psi
@Thickness 0.125 in
Injection Molded; ASTM D638
Tensile Strength, Yield 64.8 MPa
@Thickness 3.17 mm
9400 psi
@Thickness 0.125 in
Injection Molded; ASTM D638
Elongation at Yield 19 %
@Thickness 3.17 mm
19 %
@Thickness 0.125 in
Injection Molded; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 86.1 °C187 °FASTM D1525
 
Descriptive Properties
FormsPellets
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin
NOVA Chemicals Novapol® LM-2522-A LDPE Injection Molding Resin
Braskem PB 608 LDPE Injection Molding Polyethylene
Dow LDPE 955I Low Density Polyethylene
Dow LDPE 993I Low Density Polyethylene

PGLOBX20 / 42174

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.