MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taiwan Sheen Soon Sheenthane® A8970A Film Grade Thermoplastic Polyurethane Elastomer
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: Thermoplastic polyurethane elastomer for blown film

Waterproof & breathable grade

Information provided by Taiwan Sheen Soon Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85 - 8985 - 89
Tensile Strength 29.4 MPa4270 psi
Elongation at Break 550 %550 %
100% Modulus 6.85 MPa
@Strain 100 %
994 psi
@Strain 100 %
300% Modulus 12.7 MPa
@Strain 300 %
1850 psi
@Strain 300 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 190 °C320 - 374 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Taiwan Sheen Soon Sheenthane® A8556K Film Grade Thermoplastic Polyurethane Elastomer
Taiwan Sheen Soon Sheenthane® A9070A Film Grade Thermoplastic Polyurethane Elastomer
Taiwan Sheen Soon Sheenthane® A8915K Film Grade Thermoplastic Polyurethane Elastomer
Taiwan Sheen Soon Sheenthane® A8910K Film Grade Thermoplastic Polyurethane Elastomer
Taiwan Sheen Soon Sheenthane® A8670A Film Grade Thermoplastic Polyurethane Elastomer

PSHEEN915 / 156319

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.