MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Hogen Duralloy H1W 55 Tungsten/45 Copper PM Metal Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: RWMA Class 10.

Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.

Typical Resistance Welding Applications: Class 10 material is recommended as facings or inserts for projection welding electrodes and for flash and butt welding dies where high electrical conductivity is desirable and relatively high malleability is necessary. H1W and H3W are most commonly used for flash and butt welding die inserts.

Data provided by Hogen Industries.

Key Words: Hogen Industries Powder Metallurgy Metal Composite Tungsten Alloys RWMA Class 10
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density >= 12.25 g/cc>= 0.4426 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7373
Tensile Strength, Ultimate 448 MPa65000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000300 ohm-cm0.00000300 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.8 µm/m-°C
@Temperature 20.0 °C
6.56 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.251 J/g-°C
@Temperature 20.0 °C
0.0600 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 240 W/m-K
@Temperature 20.0 - 400 °C
1670 BTU-in/hr-ft²-°F
@Temperature 68.0 - 752 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 45 %45 %
Tungsten, W 55 %55 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hogen Durakut H15W 68 Tungsten/32 Copper PM Metal Composite
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite
NAECO® ELKON® R32 Tungsten Copper material ASTM B702
Hogen Duralloy H10W 75 Tungsten/25 Copper PM Metal Composite
Hogen Duralloy H30W 80 Tungsten/20 Copper PM Metal Composite

NHOG08 / 17316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.