MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allvac® Nickelvac® H-46 Specialty Steel, Heat Treatment: 1149°C (2100°F) Anneal  (discontinued **)
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Data provided by Allvac.

Applications: Structural components for land-based turbine engines. Rings and structurals in jet engines.

Key Words: Allvac, an Allegheny Teledyne Company, PWA 1091. PDS 10705Z2.
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.75 g/cc0.280 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 304304Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 330330Estimated from Rockwell C value.
Hardness, Rockwell C 3232
Hardness, Vickers 318318Estimated from Rockwell C value.
Tensile Strength, Ultimate 690 MPa100000 psi
Tensile Strength, Yield 621 MPa
@Strain 0.2 %
90100 psi
@Strain 0.2 %
Elongation at Break 18 %18 %
Reduction of Area 50 %50 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.16 %0.16 %
Chromium, Cr 11 %11 %
Copper, Cu 0.20 %0.20 %
Iron, Fe 86 %86 %as balance
Manganese, Mn 0.65 %0.65 %
Molybdenum, Mo 0.75 %0.75 %
Nickel, Ni 0.60 %0.60 %
Niobium, Nb (Columbium, Cb) <= 0.35 %<= 0.35 %
Nitrogen, N 0.040 %0.040 %
Phosphorus, P 0.010 %0.010 %
Silicon, Si 0.45 %0.45 %
Sulfur, S 0.0050 %0.0050 %
Tantalum, Ta <= 0.35 %<= 0.35 %
Vanadium, V 0.25 %0.25 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PWA 1480 Nickel Alloy Composition Spec
Goodfellow Audiolloy® Iron 52/Nickel 48 Alloy
ATI Allvac® VascoMax® C-350 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
ATI Allvac® Vasco® 17-4 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age
Weartech International WT-694 Cobalt Hardfacing & Wear Resistant Alloy

NALL84 / 14816

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.