MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GEHR Plastics PA 6 G Nylon 6, Cast, Dry  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be achieved only after conditioning, this material must be conditioned again after annealing. In addition, this conditioning occurs with a longer storage in air automatically. This is a very stress relieved and high-molecular PA 6.

Properties:

  • high impact strength and stiffness
  • high impact and notching impact strength
  • high heat deflection temperature
  • good at dampening
  • good glide and limp home characters
  • good chemical stability against organic solvents and fuels
  • size alteration by humidity absorption must be considered
  • dimension stability, electrical and mechanical properties may become affected by absorbing moisture or water
Applications include bearing parts, gear wheels, pump parts, sliding rails, castors, and fittings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccISO 1183
Water Absorption at Saturation 2.2 - 6.5 %2.2 - 6.5 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 125 - 160 MPa18100 - 23200 psiISO 2039-1
Tensile Strength, Yield 60.0 - 80.0 MPa8700 - 11600 psiISO 527
Elongation at Break 40 - 100 %40 - 100 %ISO 527
Modulus of Elasticity 1.80 - 3.10 GPa261 - 450 ksiISO 527
Flexural Strength 60.0 - 140 MPa8700 - 20300 psiISO 178
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 0.400 - 1.50 J/cm²1.90 - 7.14 ft-lb/in²ISO 179
Coefficient of Friction 0.36 - 0.420.36 - 0.42DIN 53375
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 - 1.00e+15 ohm-cm1.00e+12 - 1.00e+15 ohm-cmVDE 0303
Surface Resistance 1.00e+12 - 1.00e+13 ohm1.00e+12 - 1.00e+13 ohm
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
Dielectric Strength 20.0 - 50.0 kV/mm508 - 1270 kV/inVDE 0303
Dielectric Loss Index 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FDIN 53752
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 HBHBUL 94
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistanceyes
Bondabilityyes
CKW Resistanceno
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceyes
Resistance Against Hot Wateryes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polikim KESTAMID® PA6G Polyamide 6
Mitsubishi Chemical Advanced Materials Nylatron™ 66 SA PA66 AE Polyamide 66, extruded
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Conditioned)
Omnia Plastica Omniamid PA 6 - Akulon 6 - Dry
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide

PGEHR020 / 79857

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.