MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CHT Group QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stability. This material is an excellent choice for the molding of intricate patterns which involve deep undercuts and where dimensional stability becomes important while maintaining fairly low modulus. A variety of catalysts are offered with this material. Complies with FDA indirect food contact regulation CFR 177.2600 when used with Cat Clear FG. Refer to Cat Clear FG data sheet for specific properties.

Key Features:

  • Low viscosity
  • Excellent tear resistance
  • Fast demold time
  • Moderately high durometer with a moderately low modulus
Main Applications:
  • Molds for small statues, large statues and monument restoration
  • Molds for polyester, polyurethane and epoxy resin castings
  • Molds for prototypes
  • Picture frame and architectural molds

      Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccUncatalyzed, QM CAT RED 3
 1.00 g/cc1.00 g/ccUncatalyzed, QM CAT PURPLE
 1.03 g/cc1.03 g/ccUncatalyzed, QM CAT BLUE
 1.25 g/cc1.25 g/cccatalyzed with QM CAT PURPLE
 1.25 g/cc1.25 g/cccatalyzed with QM CAT RED 3
 1.25 g/cc1.25 g/cccatalyzed with QM CAT BLUE
 1.28 g/cc1.28 g/ccBase
Viscosity 100 cP100 cPUncatalyzed, QM CAT PURPLE
 100 cP100 cPUncatalyzed, QM CAT BLUE
 100 cP100 cPUncatalyzed, QM CAT RED 3
 15000 cP15000 cPcatalyzed with QM CAT RED 3
 15000 cP15000 cPcatalyzed with QM CAT BLUE
 15000 cP15000 cPcatalyzed with QM CAT PURPLE
 25000 cP25000 cPBase
Linear Mold Shrinkage <= 0.0030 cm/cm<= 0.0030 in/incured 72 hrs @ RT
Storage Temperature <= 38.0 °C<= 100 °F6 months
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2222cured 72 hrs @ RT
 21
@Time 86400 sec
21
@Time 24.0 hour
catalyzed with QM CAT PURPLE
 21
@Time 86400 sec
21
@Time 24.0 hour
catalyzed with QM CAT BLUE
 21
@Time 86400 sec
21
@Time 24.0 hour
catalyzed with QM CAT RED 3
Tensile Strength 2.76 MPa400 psicured 72 hrs @ RT
Elongation at Break 300 %300 %cured 72 hrs @ RT
Tear Strength 20.2 kN/m115 plicured 72 hrs @ RT
 
Processing PropertiesMetricEnglishComments
Cure Time 200 - 400 min4 - 6 hourDemold time, catalyzed with QM CAT RED 3
 720 - 960 min12 - 16 hourDemold time, catalyzed with QM CAT PURPLE
 960 - 1400 min16 - 24 hourDemold time, catalyzed with QM CAT BLUE
Tack-Free Time 45.0 - 60.0 min0.750 - 1.00 hourCatalyzed with QM CAT RED 3
 240 - 360 min4.00 - 6.00 hourCatalyzed with QM CAT PURPLE
 360 - 480 min6.00 - 8.00 hourCatalyzed with QM cat BLUE
Pot Life 7.00 min7.00 mincatalyzed with QM CAT RED 3
 35.0 min35.0 mincatalyzed with QM CAT PURPLE
 45.0 min45.0 mincatalyzed with QM CAT BLU
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorBeigeBase
 BlueUncatalyzed, QM CAT BLUE
 Light Blue catalyzed with QM CAT BLUE
 Light Purple catalyzed with QM CAT PURPLE
 Light Redcatalyzed with QM CAT RED 3
 PurpleUncatalyzed, QM CAT PURPLE
 RedUncatalyzed, QM CAT RED 3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ V-330 CA-35 Silicone Rubber
Rogers Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate
Rogers Arlon R36338R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Elkem (Bluestar Silicones) SILBIONE® LSR 4325 Liquid Silicone Rubber
DuPont Silastic® C7-4550 DICUP R Dow-Corning Biomedical Grade ETR Elastomer

PACC058 / 22185

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.