System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Micropol L20 Low density polyethylene rotational molding powder
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Low Density (LDPE)
Material Notes:
Has a high gloss finish, and outstanding toughness.
Information provided by Micropol Limited
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.916
g/cc
0.0331
lb/in³
ASTM D1505
Melt Flow
18
-
22
g/10 min
18
-
22
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
12.5
MPa
1810
psi
ASTM D638-64T
Elongation at Break
500 %
500 %
50mm/min
Flexural Modulus
0.200
GPa
29.0
ksi
ASTM D760-66
Thermal Properties
Metric
English
Comments
Vicat Softening Point
87.0
°C
189
°F
ASTM D1525
Brittleness Temperature
<=
-70.0
°C
<=
-94.0
°F
ASTM D746
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Carmel Olefins Ipethene® 830 Low Density Polyethylene
Carmel Olefins Ipethene® 810 Low Density Polyethylene
Carmel Olefins Ipethene® 670 Low Density Polyethylene
Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin
Micropol L7 Low density polyethylene rotational molding powder
PMICRO14 / 53071
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.