MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength meet all the requirements for barrier films coextrusion, even for very thin structures. The antioxidant package allows for very good thermal stability during processing. This product complies with ASTM standard D1248-IA4.

Applications: High clarity films, coextruded with polyamide, EVOH, PVdC, etc. for food packaging, such as: cheese, meat, sausages, sliced ham, etc.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 - 0.926 g/cc0.0333 - 0.0335 lb/in³ASTM D1505
Thickness 50.0 microns1.97 mil
Melt Index of Compound 0.50 - 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.50 - 0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 16.0 MPa2320 psiASTM D638
Tensile Strength, Yield 12.0 MPa1740 psiASTM D638
Film Elongation at Break, MD 350 %350 %ASTM D882
Film Elongation at Break, TD 700 %700 %ASTM D882
Elongation at Break 575 %575 %ASTM D638
Secant Modulus, MD 0.117 GPa17.0 ksi5%; ASTM D882
Secant Modulus, TD 0.125 GPa18.1 ksi5%; ASTM D882
Coefficient of Friction, Dynamic 0.550.55ASTM D1894
Elmendorf Tear Strength, MD 7.40 g/micron188 g/milASTM D1922
Elmendorf Tear Strength, TD 5.70 g/micron145 g/milASTM D1922
Dart Drop Test 160 g0.353 lb(method A); ASTM D1709
Film Tensile Strength at Break, MD 26.0 MPa3770 psiASTM D882
Film Tensile Strength at Break, TD 23.0 MPa3340 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 97.0 °C207 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 8.5 %8.5 %ASTM D1003
Gloss 90 %90 %@ 60° Gardner; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 155 - 165 °C311 - 329 °FPlasticizing Zone; Monoextrusion
 165 - 175 °C329 - 347 °FMixture Zone; Monoextrusion
 170 - 180 °C338 - 356 °FPlasticizing Zone; Coextrusion with polyamide
 180 - 190 °C356 - 374 °FMixture Zone; Coextrusion with polyamide
Feed Temperature 150 - 160 °C302 - 320 °FMono-extrusion
 160 - 170 °C320 - 338 °FCo-extrusion with Polyamide
Adapter Temperature 175 - 185 °C347 - 365 °FMono-extrusion
 220 - 230 °C428 - 446 °FCo-extrusion with Polyamide
Blow-up Ratio (BUR) 3.03.0Recommended

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyvinyl Dichloride (PVDC)
Overview of materials for PVC, Molded
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film
Overview of materials for PVC, Extruded
Inovyn 178GI Polyvinyl Chloride General Purpose - Rigid

PDAX082 / 29507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.