MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Aflux® 42 Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Processing promoter for compounds based on natural and synthetic rubbers, especially, e.g. NR, SBR, NBR, CR, and EPDM

Use: Aflux 42 acts as an excellent dispersing agent for fillers and rubber chemicals. It increases the plasticity of uncured compounds and improves the flow properties. The output and the rate of extrusion of profiles are increased. Aflux 42 imparts smooth surfaces to extrudates and calendered foils. The vulcanizate properties are practically not affected by Aflux 42

Application: For technical molded and injected articles of all types, footwear. For continuous vulcanization processes (LCM, UHF) and injection molding

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 80.0 - 100 °C176 - 212 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.5 Month36.5 Month
 
Descriptive Properties
Appearancewhite to beige Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Aktiplast® Processing Aid
Lanxess Aktiplast® 2635 Processing Aid
Lanxess Aflux® 42 M Processing Aid
Lanxess Aflux® 42 M pellets Processing Aid
Lanxess Aktiplast® T Processing Aid

PLANY8243 / 208636

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.