MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Syncon® Synthetic Transmission Oil, ISO Grade 50
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Conoco Syncon HP Synthetic Transmission Oil is a synthetic lubricant for heavy-duty manual transmissions, with or without synchronizers. It is approved by Eaton Corp. as an alternative to Eaton Roadranger Synthetic Transmission Oil. It is also appropriate for bearings and gears in industrial applications where ISO viscosity grades 150 and 220 are recommended. Syncon HP Synthetic Transmission Oil is formulated with high-quality, synthetic PAO base oils and additives to protect against rust and corrosion, oxidation and wear. Its low pour point and low-temperature viscosity make for easier cold-weather shifting. Syncon HP Synthetic Transmission Oil is an SAE 50 oil that meets API MT-1, GL-1 and Eaton PS-081 specifications. It is recommended for Classes 6, 7 and 8 manual transmissions built by Eaton Corp. (Fuller Division), Dana Corp. (Spicer Division) and others. Oil-drain intervals can be extended to as long as 500,000 miles (800,000 km).

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 23 °23 °
Viscosity 45000 cP
@Temperature -30.0 °C
45000 cP
@Temperature -22.0 °F
Viscosity Measurement 154154Viscosity Index
Kinematic Viscosity at 40°C (104°F) 138 cSt138 cSt
Kinematic Viscosity at 100°C (212°F) 18 cSt18 cSt
ASTM Color 8.08.0
 
Thermal PropertiesMetricEnglishComments
Pour Point -40.0 °C-40.0 °F
Flash Point 227 °C440 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Syncon® 22 Synthetic AW Hydraulic Fluid 22
Nye Lubricants UniFlor 8990 (UF) Synthetic Oil

WCON023 / 75060

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.