MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DIAB Klegecell® R 75 Rigid, Closed Cell PVC Foam Core Material  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Klegecell R is a PVC based, rigid, closed-cell foam with a tri-dimensional grid structure, which provides high thermal stability and structural integrity. As a structural core, Klegecell R is used in conjunction with high strength facings to produce lightweight, yet exceptionally stiff composite structures. Klegecell is widely used and found in pleasure crafts, tanks, high performance boats, vehicles, and many other high-strength, low-weight applications.

Information provided by DIAB, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0753 g/cc0.00272 lb/in³Nominal
 0.0678 - 0.08659 g/cc0.00245 - 0.003128 lb/in³Tolerance from nominal of -10%/+15%.; ISO 845
Water Vapor Transmission 5.10 g/m²/day0.328 g/100 in²/dayISO 1663
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1.90 MPa276 psiISO 1926
Elongation at Break 11 %11 %Shear Strain
Tensile Modulus 0.0620 GPa8.99 ksi
Compressive Strength 1.30 MPa189 psiISO 844
Compressive Modulus 0.10897 GPa15.805 ksiASTM D1621-B
Poissons Ratio 0.320.32
Shear Modulus 0.03099 GPa4.495 ksiISO 1922
Shear Strength 1.00 MPa145 psiISO 1922
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
19.4 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.75 J/g-°C0.418 BTU/lb-°F
Thermal Conductivity 0.0300 W/m-K
@Temperature 10.0 °C
0.208 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
ASTM C518
Insulation R Value 2.42.40.5 inch sample; based on a +10°C K factor.
 4.84.81.0 inch sample; based on a +10°C K factor.
 9.69.62.0 inch sample; based on a +10°C K factor.
Maximum Service Temperature, Air 70.0 °C158 °FContinuous
Minimum Service Temperature, Air -200 °C-328 °FContinuous
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 80.0 °C<= 176 °F
 
Descriptive Properties
Water Absorption0.012 lb/ft²ASTM C272

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CoreLite PVC 80 Closed-Cell PVC Foam Sheet
DIAB Divinycell® H 80 Sandwich Core Material
DIAB Klegecell® R 60 Rigid, Closed Cell PVC Foam Core Material
DIAB Klegecell® R 45 Rigid, Closed Cell PVC Foam Core Material
Overview of materials for PVC, Foam Grade

PDIAB28 / 29818

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.