Hostacom PPU X9067HS C11503 is an unfilled PP copolymer, with high flowability, superior stiffness and high toughness. Product is available as a customized color matched, pellet form. This grade is delivered in C11503 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Applications: Automotive Parts, Interior TrimsInformation provided by LyondellBasell. |