MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 851.0-T5, Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 851.0-T5; UNS A08510; AA851.0-T5; Al851.0-T5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.83 g/cc0.102 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 30 - 6030 - 60AA; Typical; 500 g load; 10 mm ball
Tensile Strength, Ultimate >= 117 MPa>= 17000 psiAA
Elongation at Break >= 3.0 %>= 3.0 %AA; in 2 in. (50 mm) or 4D
Tensile Modulus 71.0 GPa10300 ksiAluminum 850.0
Poissons Ratio 0.330.33Estimated from aluminum 850.0
Machinability 90 %90 %0-100 Scale (100=best)
Shear Modulus 26.5 GPa3840 ksiEstimated from aluminum 850.0
Shear Strength 75.0 MPa10900 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000400 ohm-cm0.00000400 ohm-cmAA; Typical 43% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  22.7 µm/m-°C
@Temperature 20.0 - 100 °C
12.6 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical
 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
14.2 µin/in-°F
@Temperature 68.0 - 572 °F
Estimated by MatWeb
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°FTypical for cast aluminum
Thermal Conductivity 167 W/m-K1160 BTU-in/hr-ft²-°FAA; Typical at 25°C
Melting Point 227 - 629.4 °C440 - 1165 °FAA; Typical
Solidus 227 °C440 °FAA; Typical
Liquidus 629.4 °C1165 °FAA; Typical
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 86.6 - 91.5 %86.6 - 91.5 %As remainder
Copper, Cu 0.70 - 1.3 %0.70 - 1.3 %
Iron, Fe <= 0.70 %<= 0.70 %
Magnesium, Mg <= 0.10 %<= 0.10 %
Manganese, Mn <= 0.10 %<= 0.10 %
Nickel, Ni 0.30 - 0.70 %0.30 - 0.70 %
Other, total <= 0.30 %<= 0.30 %
Silicon, Si 2.0 - 3.0 %2.0 - 3.0 %
Tin, Sn 5.5 - 7.0 %5.5 - 7.0 %
Titanium, Ti <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PCP-Canada ALCA MAX® 2XXX Cast Aluminum Mold Blocks/Plate
Aluminum 850.0-T5, Permanent Mold Cast
Aluminum 851.0-T6, Permanent Mold Cast
Overview of materials for Low Alloy Steel
Aluminum 711.0-T1, Permanent Mold Cast

MAC8510T5P / 10216

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.