MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® RL31 Polyester Film, 50 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Mylar® RL31 is commercially available in nominal 50, 75 and 100 gauges. Mylar® RL31 is designed to seal to a broad range of container substrates including amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, polyvinylchloride (PVC), polyethylene (HDPE), polypropylene (PP), and polystyrene (HIPS). Mylar® RL31 was developed as a replacement for Mylar® RL2 with improved grease and oil resistance, and has been shown to be superior in almost all applications. Heat seals with Mylar® RL31 are stronger than with Mylar® OL, but are still generally strippable from most container substrates. Shredding (film tear or break) can be minimized or eliminated by using higher gauges. Mylar® RL31 has a lower seal initiation temperature than lidding films with an amorphous polyester heat seal layer (e.g., Mylar® OL, OL2). This allows good seals to be made at higher line speeds (or using lower sealing temperatures). Mylar® RL31 is not recommended for applications where "caulking" is required. Mylar® RL31 can withstand freezing temperatures down to -40°F, and foods can be heated or cooked in contact with this film at temperatures up to 400°F. The oriented polyester base film will begin to distort in the range of 425-450°F.

Corona Treatment (Mylar® RL31T): Selected gauges of Mylar® RL31 are available with corona treatment (on the opposite side of film from the heat seal layer) to enhance printing and laminating. This film type is marketed by DuPont Teijin Films as Mylar® RL31T and is commercially available in nominal 50, 75, and 100 gauges. The film is treated to an initial dyne level of 54. The dyne level of treated lidding films may decline with storage, and in-line corona treatment may be required during subsequent printing or laminating to increase the dyne level to a value adequate to get desired ink or laminate adhesion. Standard put-ups for Mylar® RL31T are the same as shown for Mylar® RL31. Anti-fog: Mylar® RL31 is not available with anti-fog capability.

Approvals: FDA Food Contact Status - All gauges of Mylar® RL31 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Mylar® RL31 can be used to contain foods during oven cooking or oven baking at temperatures above 250°F.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³Typical Mylar®; ASTM D1505
Water Vapor Transmission 20.2 g/m²/day
@Temperature 38.0 °C
1.30 g/100 in²/day
@Temperature 100 °F
90% RH; ASTM F1249
Thickness 12.7 microns0.500 mil
Coating Weight 20.3 g/m²12.7 lb/ream0.5 m2; ASTM E252
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 110 %110 %ASTM D882A
Film Elongation at Break, TD 80 %80 %ASTM D882A
Tensile Modulus 3.79 GPa550 ksiASTM D882
Graves Tear Strength 0.123 kN/m0.700 pliASTM D1004
Film Tensile Strength at Break, MD 172 MPa25000 psiASTM D882A
Film Tensile Strength at Break, TD 241 MPa35000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Gas Permeability (Base film)5 cc/100 in2O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal)19500 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® OWF2 Polyester Film, 60 Gauge
DuPont Teijin Films Mylar® WC Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® RL31 Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® RB42AF Polyester Film, 100 Gauge
DuPont Teijin Films Mylar® RSX Polyester Film, 48 Gauge

PDTZ9399 / 139719

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.