MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Clariant Renol PEEKSP003 Polyetheretherketone, Glass Fiber, PTFE Lubricated  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled; Polyetheretherketone, PEEK, PTFE-Filled

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 155 MPa22500 psiASTM D638
Flexural Yield Strength 241 MPa35000 psiASTM D790
Flexural Modulus 11.0 GPa1600 ksiASTM D790
Izod Impact, Notched 1.07 J/cm
@Temperature 22.8 °C
2.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 349 - 399 °C660 - 750 °F
Mold Temperature 163 - 218 °C325 - 425 °F
Dry Time <= 3 hour
@Temperature 149 °C
<= 3 hour
@Temperature 300 °F
to ensure moisture level is below 0.1%
Injection Pressure 49.6 - 74.5 MPa7200 - 10800 psiSecondary
 82.7 - 124 MPa12000 - 18000 psiInitial
Back Pressure 0.000 - 0.345 MPa0.000 - 50.0 psi
Shot Size 30 - 80 %30 - 80 %
Screw Speed 20 - 50 rpm20 - 50 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Akro-Plastic Akrotek® PEEK GF 50 natural (5100) PEEK, Conditioned, 50% Glass Filled
Akro-Plastic Akrotek® PEEK GF 50 natural (5100) PEEK, Dry, 50% Glass Filled
Akro-Plastic Akrotek® PEEK GF 60 9 natural (5184) PEEK, Conditioned, 60% Glass Filled
Akro-Plastic Akrotek® PEEK natural (5184) PEEK, Conditioned

PCLAR165 / 82290

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.