MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis FS1560 High Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and balanced tear properties. Applications FS1560 has been developed especially for applications like: heavy-duty sacks, refuse sacks and liners, and carrier-bag film. FS1560 contains antioxidant.

Information provided by Borealis AG

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³ISO 1183
Melt Flow  0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 250 %250 %ISO 527-3
Film Elongation at Break, TD 300 %300 %ISO 527-3
Tensile Modulus 1.00 GPa145 ksiMD; ASTM D882-A
 1.10 GPa160 ksiTD; ASTM D882-A
Puncture Energy 1.50 J1.11 ft-lb45N; ASTM D5748
Elmendorf Tear Strength MD 20.387 g20.387 gISO 6383/2
Elmendorf Tear Strength TD 30.58 g30.58 gISO 6383/2
Dart Drop Test 350 g0.772 lbISO 7765-1
Film Tensile Strength at Break, MD 50.0 MPa7250 psiISO 527-3
Film Tensile Strength at Break, TD 55.0 MPa7980 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °FISO 11357-3
Vicat Softening Point 127 °C261 °FISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 230 °C410 - 446 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Borealis FG5224 Linear Low Density Polyethylene
Baystar™ 2285 HDPE Bimodal Film Resin
Borealis HD234CF Polypropylene
Formosa Plastics Formolene® E927 Film HDPE

PBOREA451 / 108710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.