MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Potassium Chloride, KCl (Sylvite)
Categories: Ceramic; Halide

Material Notes: White cubic crystals

Key Words: Potassium Chloride
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.988 g/cc0.07182 lb/in³
Solubility in Water 35.5 %
@Temperature 25.0 °C
35.5 %
@Temperature 77.0 °F
a Lattice Constant 6.2931 Å6.2931 Å
Formula Units/Cell (Z) 44
Molecular Weight 74.551 g/mol74.551 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.02.0
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.0000388-0.0000388cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 355.9 J/g153.1 BTU/lb
Melting Point 771 °C1420 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49
@Wavelength 589.3 nm
1.49
@Wavelength 589.3 nm
η, Na
 
Descriptive Properties
CAS Number7447-40-7
ColorWhite
Crystal StructureCubicRock salt

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mateck Potassium Chloride (KCl)
Sodium Chloride, NaCl (Halite)
Magnesium Chloride, MgCl2 (Chloromagnesite)
Calcium Chloride, CaCl2
Mateck Zinc Sulfide Cleartran (ZnS)

EINOR0626 / 3758

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.