MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Cetus® DE 100
Categories: Fluid; Lubricant

Material Notes: Texaco Cetus DE oils deliver value through:
  • Long life — Texaco Cetus DE oils have a low sludge-forming tendency and a high solvency for deposits that help to keep compressor parts clean. Their ability to reduce oil consumption and carry over; reduce varnish, sludge, and deposits; as well as increase deposit-free valve life translates to reducing compressor maintenance and energy costs.
  • Ignition safety — Texaco Cetus DE oils provide a greater margin of safety than conventional petroleum products because their flash points, fire points, and auto ignition temperatures are much higher. They are not, however, true fire resistant fluids.

Texaco Cetus DE oils are synthetic diester-based, oxidation resistant, compressor oils.

Texaco Cetus DE oils are used for portable and stationary rotary screw, rotary vane, and reciprocating compressors. While specific manufacturer recommendations vary, the ISO 68 grade is most commonly used for rotary compressors, while higher viscosity grades are preferred for reciprocating units.

These oils can be used in compressors with the following gases: process air, benzene, butadiene, carbon dioxide (dry), carbon monoxide, ethylene, furnace (crack) gas, helium, hydrocarbon gases, hydrogen, inert gases, methane, natural gas, nitrogen, propane, sulfur hexafluoride, and synthesis gas. Texaco Cetus DE oils can be used in contact with the following seals, paints, and plastics: Viton®1, High nitrile Buna N, Teflon®2, Epoxy paint, Oil-resistant alkyd, Nylon, Delrin®3, Celcon®4, These oils should not be used with: Neoprene, SBR rubber, Low nitrile Buna N, Acrylic paint, Lacquer, Polystyrene, PVC, ABS. Do not use in breathing air apparatus or medical equipment.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222079; MSDS Number: 8713

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 15.9 °15.9 °
Viscosity Measurement 8484Viscosity Index
Saybolt Viscosity at 100°F 518 SUS518 SUS
Saybolt Viscosity at 210°F 61.7 SUS61.7 SUS
Kinematic Viscosity at 40°C (104°F) 98.8 cSt98.8 cSt
Kinematic Viscosity at 100°C (212°F) 10.4 cSt10.4 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -35.0 °C-31.0 °F
Flash Point 240 °C464 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Sheet Grade
Overview of materials for PVC, Molded
Overview of materials for PVC, High Impact
ChevronTexaco Syntholube® ISO 32 Compressor Oil
ChevronTexaco 128 Refined Wax

WTEXA041 / 76920

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.