MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

The NanoSteel® Company SHS 9800 Steel Alloy, Wear Plate
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Coating Description: SHS 9800 is a patented iron based glass forming steel alloy with a near nanoscale (submicron) microstructure that includes chromium, molybdenum and niobium in the material chemistry, resulting in an overlay wear solution well suited for the toughest jobs in the most extreme service environments.

    Key Performance Characteristics
  • 68 - 71 HRc single and double pass weld deposits
  • Maintains high hardness after exposure to high temperatures
  • Exceptional resistance to severe sliding abrasion
  • Toughness equivalent to 400 Brinell Q&T plate
  • Forming/cutting response similar to standard chrome carbide plate

Application Process: Weld Overlay for Wear Plate and Hardfacing

Information Provided by The NanoSteel Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.36 g/cc0.266 lb/in³Deposit Property
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 68 - 7168 - 71
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 10 %<= 10 %
Carbon, C <= 2.0 %<= 2.0 %
Chromium, Cr <= 25 %<= 25 %
Iron, Fe >= 33 %>= 33 %
Manganese, Mn <= 5.0 %<= 5.0 %
Molybdenum, Mo <= 10 %<= 10 %
Niobium, Nb (Columbium, Cb) <= 10 %<= 10 %
Silicon, Si <= 5.0 %<= 5.0 %
 
Descriptive Properties
Impact ResistancePassed multiple impacts at 165 ft-lbsDrop Impact Testing
Wear Resistance Mass Loss (g)0.09-0.136000 cycles; ASTM G65-04 Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trimay® Wear Plate T171 Iron-based Steel Overlay
The NanoSteel® Company SHS 9700 Steel Alloy, Wear Plate
AMG Aluminum Tibor® 10% Ti - 1% B Titanium Boron Aluminum Alloy
AMG Aluminum Boral® 10% Boron Aluminum Alloy
AMG Aluminum 50% Silicon Aluminum Alloy

NNANO019 / 106814

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.