MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PSM Industries PM Krupp T-42 Powder Metallurgy Steel Alloy
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel

Material Notes: PSM Industries is a company that is using Powder Metallurgy technologies to create engineered materials for applications requiring extreme wear resistance and toughness. The drive is to use conventional Powder Metallurgy tooling to capture net or near net shapes in materials that were previously were ingot-cast wrought products. By capturing more net shape, the result is that the number of costly secondary labor operations are reduced which translates to lower manufacturing costs.

Information Provided by PM Krupp, a division of PSM Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 66 - 6866 - 68
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.3 %1.3 %
Chromium, Cr 4.2 %4.2 %
Cobalt, Co 10.25 %10.25 %
Iron, Fe 67.15 %67.15 %As Balance
Molybdenum, Mo 3.8 %3.8 %
Tungsten, W 10 %10 %
Vanadium, V 3.3 %3.3 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PSM Industries PM Krupp A11 MOD Powder Metallurgy Steel Alloy
PSM Industries PM Krupp D-2 Powder Metallurgy Steel Alloy
PSM Industries PM Krupp M-2 Powder Metallurgy Steel Alloy
PSM Industries PM Krupp M3/2 Powder Metallurgy Steel Alloy
PSM Industries PM Krupp M4 Powder Metallurgy Steel Alloy

NPSM033 / 93224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.