MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Corning 9010 Alkali Barium Crushed Glass
Categories: Ceramic; Glass

Material Notes: Used for sealing and other applications.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.64 g/cc0.0954 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.90 µm/m-°C
@Temperature 0.000 - 300 °C
4.94 µin/in-°F
@Temperature 32.0 - 572 °F
Softening Point 646 °C1190 °F
Annealing Point 445 °C833 °F
Strain Point 405 °C761 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corning 9013 Alkali Barium Crushed/Powdered Glass
Ametek Tungsten-Copper Composites AWC 9010
H.C. Starck WCu 90/10 Tungsten-Copper Composite Material
MarkeTech W90Cu Tungsten/Copper Heat Sink Material
Kinetics MIM F15 (Kovar™) Low CTE Alloy

CCORNG11 / 742

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.