MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Schott S8806A Contrast Enhancement Filter
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Contrast Enhancement Filter

Information Provided by SCHOTT North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.50 g/cc0.126 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.20 µm/m-°C
@Temperature 20.0 - 300 °C
4.00 µin/in-°F
@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 645 °C1190 °F
Softening Point 734 °C1350 °F
Working Point 804 °C1480 °F
Annealing Point 651 °C1200 °F
Strain Point 635 °C1180 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.688
@Wavelength 587.6 nm
1.688
@Wavelength 587.6 nm
nd, Sodium
Transmission, Visible  0.40 %
@Wavelength 580 nm
0.40 %
@Wavelength 580 nm
 62 %
@Wavelength 445 nm
62 %
@Wavelength 445 nm
 67 %
@Wavelength 550 nm
67 %
@Wavelength 550 nm
 82.3 %
@Wavelength 618 nm
82.3 %
@Wavelength 618 nm
 
Descriptive Properties
ColorViolet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott S8801 Contrast Enhancement Filter
Schott S8807 Contrast Enhancement Filter

CSGS107 / 93441

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.