MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Description

CP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact.
Application

CP 810-01 meets the specifications contained in FDA Regulation CFR 177.1520(c)3.1.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.926 g/cc0.926 g/ccASTM D792
ESCR 100% Igepal® >= 50 hour>= 50 hourCondition C; ASTM D1693
Melt Index of Compound 33 g/10 min
@Load 2.16 kg,
Temperature 190 °C
33 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5353ASTM D2240
Tensile Strength, Yield 13.1 MPa1900 psi2"/min; ASTM D638
Elongation at Break 120 %120 %2"/min; ASTM D638
Flexural Modulus, 1% Secant 414 MPa60000 psiASTM D790
Falling Dart Impact 27.1 J
@Temperature -40.0 °C
20.0 ft-lb
@Temperature -40.0 °F
ASTM 3029
 
Processing PropertiesMetricEnglishComments
Melt Temperature 95.0 °C203 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman CP814-01 Linear, Low-Density Polyethylene
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
A. Schulman CP80-01 Linear Low-Density Polyethylene
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin

PASHU071 / 25035

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.