MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® FP-EF-105 PTFE, 25% Glass Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Description: Fluon® FP-EF-105 (464 102 520) is a 25% glass reinforced ETFE product designed for use in injection molding or extrusion applications. The glass fibers are added to improve the physical properties of ETFE. This compound is supplied in cylindrical pellet form. These pellets are approximately 0.125” long by 0.100” diameter.

End Uses: Demanding applications where the thermal and chemical resistance of ETFE is required with additional mechanical toughness provided by glass-fiber addition.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.89 g/cc1.89 g/ccASTM D792
Bulk Density 0.860 g/cc0.0311 lb/in³ASTM D1895
Filler Content 25 %25 %
Melt Flow 3.5 g/10 min3.5 g/10 minASTM D2116
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.2 MPa8000 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 103 MPa15000 psiASTM D790
Flexural Modulus 4.83 GPa701 ksiASTM D790
Izod Impact, Notched 3.20 J/cm6.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® FC 405 PTFE, 25% Glass Fiber Filled
AGC Fluon® RB1025S 25% Glass Fiber, PTFE Filled Compound
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Beijing Evergrow Resources PTFE, 25% Glass Fiber Filled
AGC FC 405 PTFE, 25% Glass Fiber

PAGCX131 / 191240

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.