MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kraton® D1101 K (SBS) Liner Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Kraton D1101 K is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified:
Kraton D1101 KT - supplied as a dusted porous pellet
Kraton D1101 KU - supplied as an undusted porous pellet
Kraton D1101 KIM - supplied as a dusted powder

Region: Asia Pacific, Europe, Japan, North America and South America

Uses: Kraton D1101 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It may also find use as an ingredient in formulating adhesives, sealants and coatings.

Note 1: The final dusting level is a combination of the talc from the original D1101 KT plus calcium carbonate added during the milling process.

Applications: Bitumen Modification; Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D402
Volatiles <= 0.70 %<= 0.70 %KM 04
Viscosity 3900 cP3900 cP25% Toluene Solution at 25°C; BAM 922
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Ash 0.15 - 0.35 %0.15 - 0.35 %KT, Talc; BAM 908
 4.0 - 6.0 %4.0 - 6.0 %KIM, See note 1; BAM 908
 
Chemical PropertiesMetricEnglishComments
Diblock Content 16 %16 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 69
@Time 10.0 sec
69
@Time 0.00278 hour
Typical values on polymer compression molded at 350°F; ASTM D2240
Tensile Strength 31.7 MPa4600 psimeasured on films cast from a solution in toluene; ASTM D412
Elongation at Break 880 %880 %Measured on films cast from a solution in toluene; ASTM D412
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.15-0.4%, KM 08
 Polystyrene39-33%, KM 03
 Total Extractables<1.0%, KM 05
Styrene/Rubber Ratio31/69

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® FG1901 + PA-6 blend (20/80)
Kraton® FG1901 + PBT blend (30/70)
Kraton® G1702 + PPE blend (20/80)
Kraton® D1102 B (SBS) Liner Block Copolymer
Kraton® D1101 E (SBS) Liner Block Copolymer

PKRA9807 / 132706

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.