MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Herculoy®, High-Silicon Bronze A, UNS C65500, H04 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability. Fabricated by blanking, drawing, forming and bending, heading and upsetting, hot forging and pressing, roll threading and knurling, shearing, squeezing, and swaging.

Applications: hydraulic pressure lines, anchor screws, bolts, cable clamps, cap screws, machine screws, marine hardware, nuts, pole-line hardware, rivets, U-bolts, electrical conduits, heat exchanger tubing, welding rod, propeller shafts.

Test specimen: flat products - 1mm thickness.

Key Words: HCDA 655, CS101, ISO CuSi3Mn1, CEN CS101, copper-silicon, silicon bronze
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.53 g/cc0.308 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 9393
Tensile Strength, Ultimate 650 MPa94300 psi
Tensile Strength, Yield 400 MPa
@Strain 0.5 %
58000 psi
@Strain 0.5 %
Elongation at Break 8.0 %8.0 %In 50 mm
Modulus of Elasticity 105 GPa15200 ksi
Poissons Ratio 0.3460.346
Fatigue Strength 200 MPa
@# of Cycles 1.00e+8
29000 psi
@# of Cycles 1.00e+8
Reverse Bending
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Forgeability 40 %40 %UNS C37700 (forging brass) = 100%
Shear Modulus 39.0 GPa5660 ksi
Shear Strength 390 MPa56600 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000246 ohm-cm
@Temperature 20.0 °C
0.0000246 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 36.0 W/m-K250 BTU-in/hr-ft²-°F
Melting Point 970 - 1025 °C1780 - 1877 °F
Solidus 970 °C1780 °F
Liquidus 1025 °C1877 °F
Annealing Point 482 - 704 °C900 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 475 - 700 °C887 - 1290 °F
Hot-Working Temperature 700 - 875 °C1290 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 97 %97 %
Iron, Fe <= 0.80 %<= 0.80 %
Lead, Pb <= 0.50 %<= 0.50 %
Manganese, Mn <= 1.5 %<= 1.5 %
Nickel, Ni <= 0.60 %<= 0.60 %
Silicon, Si 2.8 - 3.8 %2.8 - 3.8 %
Zinc, Zn <= 1.5 %<= 1.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Free-cutting phosphor bronze, UNS C54400, H04 Temper 25 mm rod
Dezincification Brass, DZR, UNS C35330
Low-silicon bronze B, UNS C65100, H04 (36%) Temper rod
Mueller Ecostream™ GreenDrop™ C27451 DZR Lead Free Plumbing Brass
Low-silicon bronze B, UNS C65100, OSO35 Temper rod

MC65500c1 / 11659

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.