MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MarkeTech Yttrium aluminum garnet:Ce (YGA:Ce; Y3Al5O12) Scintillator Crystal  (discontinued **)
Categories: Ceramic; Oxide

Material Notes: Yttrium aluminum garnet activated by cerium is fast with excellent mechanical properties and is chemically resistant scintillator. Mechanical properties enable to produce YAG:Ce scintillation screens down to a thickness of 30 µm. YAG:Ce detectors are excellent for electron microscopy, beta and X-ray counting, electron and X-ray imaging screens.

Data provided by MarkeTech International. MarkeTech International is no longer in business.

Key Words: Y3Al5O12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.57 g/cc0.165 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 8.58.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 - 9.00 µm/m-°C4.44 - 5.00 µin/in-°F
Melting Point 1970 °C3580 °F
 
Descriptive Properties
Crystal StructureCubic
Hydroscopic?No
Luminescence: Afterglow<0.005%at 6 ms
Luminescence: Decay Constant70 n/s
Luminescence: Integrated Light Output15NaI:Tl = 100
Luminescence: Photon Yield8300K; 103 pH/MeV
Luminescence: Radiation Length3.5 cm
Luminescence: Wavelength of max emissions550 nm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Yttrium Aluminum Oxide, Y3Al5O12
SAES Getters Nd:YAG Solid State Laser Crystals (Nd-doped Y3Al5O12)
Barium Aluminate, BaAl2O4
MarkeTech Yttrium aluminum perovskite:Cerium (YAP:Ce; YAlO3) Scintillator Crystal
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3

C5MT837 / 120746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.