MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled; Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes:

Information provided by Asia International Enterprise (Hong Kong) Ltd.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc
@Temperature 23.0 °C
1.51 g/cc
@Temperature 73.4 °F
ASTM D792
Filler Content 15 %15 %
Linear Mold Shrinkage 0.0050 - 0.012 cm/cm0.0050 - 0.012 in/inASTM D955
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 250 °C
19 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 98.1 MPa14200 psi5mm/min; ASTM D638
Elongation at Break 4.0 %4.0 %5mm/min; ASTM D638
Flexural Strength 152 MPa22000 psi2.8mm/min; ASTM D790
Flexural Modulus 5.88 GPa853 ksi2.8mm/min; ASTM D790
Izod Impact, Notched 0.588 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 230 - 265 °C446 - 509 °FCylinder Temperature
Mold Temperature 50.0 - 100 °C122 - 212 °F
Drying Temperature 120 - 140 °C248 - 284 °F
Dry Time 3 - 5 hour3 - 5 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asia International Enterprise (Hong Kong) 3010F Polybutylene terephthalate
Asia International Enterprise (Hong Kong) 30G6F Polybutylene terephthalate, 30% Glass Fiber Filled
Asia International Enterprise (Hong Kong) 30G6 Polybutylene terephthalate, 30% Glass Fiber Filled
Asia International Enterprise (Hong Kong) 30G3 Polybutylene terephthalate, 15% Glass Fiber Filled
Asia International Enterprise (Hong Kong) 3010FW Polybutylene terephthalate

PHKI002 / 108354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.