MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmocoll® 406 Polyurethane Adhesive
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Predominantly linear hydroxyl polyurethane. Desmocoll® 406 is a flexible polyurethane with a low crystallization rate. It has outstanding adhesion on flexibilised PVC and can be used to formulate adhesives with a long tack life.

Properties / Applications: Desmocoll® 406 is suitable for the formulation of adhesives for use on various materials, e.g. leather, rubber, textiles, wood, many plastics (including PU elastomers), plastic films and aluminum foils.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccDIN EN ISO 2811
Viscosity 400 - 800 cP400 - 800 cP15% in butanone-2 (MEK) at 23 °C, Haake; DIN EN ISO 3219/A.3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 °C50.0 °Factivation temp; DIN EN 12961
 
Descriptive Properties
Content<0.1%Hydroxyl, DIN 53 240
Crystallization72[h], DIN 53 505
Heat resistance40[°C], ASTM D816
Hot tack life4[min], DIN EN 12961

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmocoll® 140 Polyurethane Adhesive
Covestro Desmocoll® 500/2 Polyurethane Adhesive
Covestro Desmocoll® 400/2 Polyurethane Adhesive
Covestro Desmocoll® 176 Polyurethane Adhesive
Covestro Desmocoll® 540/1 Polyurethane Adhesive

PCOVEST0282 / 202065

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.