MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nanocyl PLASTICYL™ PP2001 Polypropylene with 2 wt% Multi-Wall Carbon Nanotubes
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Carbon Fiber Filled

Material Notes: PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PP2001 is a conductive masterbatch based on polypropylene. Because of its low viscosity and high flow formulation, PLASTICYL™ PP2001 is ideal for standard injection molding and extrusion processes.

Key Applications:

  • ESD (Electrostatic Discharge) and electrically conductive parts
  • E&E automotive and industrial
  • Injection molding, extrusion

Benefits:

  • Electrical conductivity at low loading
  • Retention of key mechanical properties
  • Easier processing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 2 %2 %Carbon Nanotube Loading
Melt Flow 5.6 g/10 min5.6 g/10 minISO 1133:1997
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.5 MPa5150 psiISO 527-1,2
Elongation at Break 154 %154 %ISO 527-1,2
Tensile Modulus 1.728 GPa250.6 ksiISO 527-1,2
Charpy Impact, Notched 0.320 J/cm²1.52 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.10e+6 ohm-cm4.10e+6 ohm-cmCTM E043
Surface Resistivity per Square 6.10e+10 ohm6.10e+10 ohmCTM E042
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FMasterbatch; ISO 11357-1,-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nanocyl PLASTICYL™ PP2001 Polypropylene with 1 wt% Multi-Wall Carbon Nanotubes

PNANOCY975 / 108930

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.