MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Echo® RPPC 20/10 BK Recycled Polypropylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Copolymer Polypropylene, Unreinforced, 20 MFI, 10 Izod, Black

Entecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.

Information provided by Entec.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break 240 %240 %ASTM D638
Elongation at Yield 11 %11 %ASTM D638
Flexural Strength 18.0 MPa2610 psi50N; ASTM D790
Flexural Modulus, 1% Secant 848 MPa123000 psiASTM D790
Izod Impact, Notched 5.33 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
9.99 ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C163 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C115 °FASTM D648
Vicat Softening Point 59.0 °C138 °FASTM D 1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Echo® RPPC 20/2 BK Recycled Polypropylene
Buckeye Polymers BP RPPC 1020 TU BLK Polypropylene Copolymer
Ravago Manufacturing Americas Echo® RPPC 20/6 BK Polypropylene Copolymer
Bamberger Polymers Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade
Buckeye Polymers BP RPPC 0510 Blk Reprocessed Polypropylene, Unfilled

PENTA014 / 36020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.