MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shin-Etsu Silicones KE-1820 Silicone, RTV Adhesive/Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes:

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545
Tensile Strength 5.40 MPa783 psi
 
Electrical PropertiesMetricEnglishComments
Dissipation Factor 0.0050
@Frequency 50 Hz
0.0050
@Frequency 50 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 120 °C
1.00 hour
@Temperature 248 °F
 
Descriptive Properties
ColorsWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-1830 Silicone, RTV Adhesive/Sealant
Dow Q2-7735 ADHESIVE
Dow 734 FLOWABLE SEALANT
Momentive Performance Materials TSE3221 Clear Adhesive Sealant, Non-Corrosive Flowable
Shin-Etsu Silicones C-19A Silicone Gum

PSHIN284 / 177795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.