MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ohara S-FPL51Y i-Line Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes: i-Line High Homogeneity Glass. ECO optical glass that does not contain any lead or arsenic.

Information provided by Ohara Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.66 g/cc3.66 g/cc
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 5151
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 380
@Load 0.0999 kg
380
@Load 0.220 lb
Modulus of Elasticity 71.6 GPa10400 ksi
Modulus of Rigidity 27.5 GPa3990 ksi
Poissons Ratio 0.3020.302
Abrasion 476476Aa
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.6 µm/m-°C
@Temperature -30.0 - 70.0 °C
7.56 µin/in-°F
@Temperature -22.0 - 158 °F
 16.1 µm/m-°C
@Temperature 100 - 300 °C
8.94 µin/in-°F
@Temperature 212 - 572 °F
Thermal Conductivity 0.780 W/m-K
@Temperature 35.0 °C
5.41 BTU-in/hr-ft²-°F
@Temperature 95.0 °F
Transformation Temperature, Tg 448 °C838 °Fper thermal expansion curve
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.47980
@Wavelength 2325.42 nm
1.47980
@Wavelength 2325.42 nm
 1.48286
@Wavelength 1970.09 nm
1.48286
@Wavelength 1970.09 nm
 1.48617
@Wavelength 1529.58 nm
1.48617
@Wavelength 1529.58 nm
 1.48913
@Wavelength 1128.64 nm
1.48913
@Wavelength 1128.64 nm
 1.49011
@Wavelength 1013.98 nm
1.49011
@Wavelength 1013.98 nm
nt (Hg t line)
 1.49182
@Wavelength 852.11 nm
1.49182
@Wavelength 852.11 nm
ns (Cs s line)
 1.49299
@Wavelength 768.19 nm
1.49299
@Wavelength 768.19 nm
nA' (K A' line)
 1.49407
@Wavelength 706.52 nm
1.49407
@Wavelength 706.52 nm
nr (He r line)
 1.49513
@Wavelength 656.27 nm
1.49513
@Wavelength 656.27 nm
nC (H C line)
 1.49543
@Wavelength 643.85 nm
1.49543
@Wavelength 643.85 nm
nC' (Cd C' line)
 1.49571
@Wavelength 632.8 nm
1.49571
@Wavelength 632.8 nm
nHe-Ne
 1.49695
@Wavelength 589.29 nm
1.49695
@Wavelength 589.29 nm
nD (Na D line)
 1.49700
@Wavelength 587.56 nm
1.49700
@Wavelength 587.56 nm
nd (He D line)
 1.49847
@Wavelength 546.07 nm
1.49847
@Wavelength 546.07 nm
ne (Hg e line)
 1.50126
@Wavelength 486.13 nm
1.50126
@Wavelength 486.13 nm
nf (H F line)
 1.50160
@Wavelength 479.99 nm
1.50160
@Wavelength 479.99 nm
nF' (Cd F' line)
 1.50412
@Wavelength 441.57 nm
1.50412
@Wavelength 441.57 nm
nHe-Cd
 1.50455
@Wavelength 435.835 nm
1.50455
@Wavelength 435.835 nm
ng (Hg g line)
 1.50727
@Wavelength 404.656 nm
1.50727
@Wavelength 404.656 nm
nh (Hg h line)
 1.51185
@Wavelength 365.015 nm
1.51185
@Wavelength 365.015 nm
ni (Hg i line)
 1.51673
@Wavelength 334 nm
1.51673
@Wavelength 334 nm
 1.51826
@Wavelength 326 nm
1.51826
@Wavelength 326 nm
Abbe Number 80.7480.74ν e
 81.1481.14ν d
Optical Dispersion 0.0061250.006125nF-nC
 0.0061740.006174nF'-nC'
Transmission, Visible  99.9 %
@Wavelength 380 nm
99.9 %
@Wavelength 380 nm
 99.9 %
@Wavelength 390 nm
99.9 %
@Wavelength 390 nm
 99.9 %
@Wavelength 400 nm
99.9 %
@Wavelength 400 nm
 99.9 %
@Wavelength 420 nm
99.9 %
@Wavelength 420 nm
 99.9 %
@Wavelength 440 nm
99.9 %
@Wavelength 440 nm
 99.9 %
@Wavelength 460 nm
99.9 %
@Wavelength 460 nm
 99.9 %
@Wavelength 480 nm
99.9 %
@Wavelength 480 nm
 99.9 %
@Wavelength 500 nm
99.9 %
@Wavelength 500 nm
 99.9 %
@Wavelength 550 nm
99.9 %
@Wavelength 550 nm
 99.9 %
@Wavelength 600 nm
99.9 %
@Wavelength 600 nm
 99.9 %
@Wavelength 650 nm
99.9 %
@Wavelength 650 nm
 99.9 %
@Wavelength 700 nm
99.9 %
@Wavelength 700 nm
IR Transmittance  99.5 %
@Wavelength 2400 nm
99.5 %
@Wavelength 2400 nm
 99.6 %
@Wavelength 2200 nm
99.6 %
@Wavelength 2200 nm
 99.8 %
@Wavelength 1000 nm
99.8 %
@Wavelength 1000 nm
 99.8 %
@Wavelength 1200 nm
99.8 %
@Wavelength 1200 nm
 99.8 %
@Wavelength 1800 nm
99.8 %
@Wavelength 1800 nm
 99.9 %
@Wavelength 800 nm
99.9 %
@Wavelength 800 nm
 99.9 %
@Wavelength 900 nm
99.9 %
@Wavelength 900 nm
 99.9 %
@Wavelength 1400 nm
99.9 %
@Wavelength 1400 nm
 99.9 %
@Wavelength 1600 nm
99.9 %
@Wavelength 1600 nm
UV Transmittance  4.0 %
@Wavelength 240 nm
4.0 %
@Wavelength 240 nm
 7.0 %
@Wavelength 250 nm
7.0 %
@Wavelength 250 nm
 21 %
@Wavelength 260 nm
21 %
@Wavelength 260 nm
 34 %
@Wavelength 270 nm
34 %
@Wavelength 270 nm
 51 %
@Wavelength 280 nm
51 %
@Wavelength 280 nm
 67 %
@Wavelength 290 nm
67 %
@Wavelength 290 nm
 80 %
@Wavelength 300 nm
80 %
@Wavelength 300 nm
 89 %
@Wavelength 310 nm
89 %
@Wavelength 310 nm
 94.3 %
@Wavelength 320 nm
94.3 %
@Wavelength 320 nm
 97.1 %
@Wavelength 330 nm
97.1 %
@Wavelength 330 nm
 98.6 %
@Wavelength 340 nm
98.6 %
@Wavelength 340 nm
 99.4 %
@Wavelength 350 nm
99.4 %
@Wavelength 350 nm
 99.6 %
@Wavelength 360 nm
99.6 %
@Wavelength 360 nm
 99.7 %
@Wavelength 365 nm
99.7 %
@Wavelength 365 nm
 99.8 %
@Wavelength 370 nm
99.8 %
@Wavelength 370 nm
 
Descriptive Properties
Acid Resistance, Powder Method, RAP)4
coloring, λ 5-
coloring, λ 80310
Knoop Hardness Class4
Melt Frequency5
Ohara Code d497811
Ohara Code e498808
Ohara StatusStandard
Phosphate Resistance, PR4.2
Relative Price42.5S-BSL7 = 1
Water Resistance, RW(P)1
Weathering Resistance (Surface Method) W(S)max2
Weathering Resistance (Surface Method) W(S)min3
Yield Point, At (°C)471per thermal expansion curve

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ohara PBL25Y i-Line Optical Glass
Schott AF 45 Thin Borosilicate Glass
Ohara L-BBH1 Low Tg Optical Glass

CZOHARA869 / 192077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.