MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LL 1107x95 Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and drawability make them excellent for many film applications.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: 3500 ppm
  • Slip: 1700 ppm
  • Processing Aid: Yes
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Garment Film
  • Produce Bags
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ExxonMobil Method
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.66 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 3500 ppm3500 ppm
Slip Level 1700 ppm1700 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.3 MPa1500 psiASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiASTM D882
Film Elongation at Break, MD 520 %520 %ASTM D882
Film Elongation at Break, TD 690 %690 %ASTM D882
Puncture Energy 1.05 J0.775 ft-lbExxonMobil
Elmendorf Tear Strength, MD 2.76 g/micron70.0 g/milASTM D1922
Elmendorf Tear Strength, TD 17.3 g/micron440 g/milASTM D1922
Dart Drop 2.36 g/micron60.0 g/milASTM D1709
Film Tensile Strength at Break, MD 45.8 MPa6640 psiASTM D882
Film Tensile Strength at Break, TD 27.2 MPa3940 psiASTM D882
1% Secant Modulus, MD 230 MPa33400 psiASTM D882
1% Secant Modulus, TD 261 MPa37800 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 18.4 %18.4 %ASTM D1003
Gloss 46 %46 %45°; ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil C4LL 0822.95 Linear Low Density Polyethylene Resin
ExxonMobil LL 3201.69 Premium High Strength Film Resin
ExxonMobil LL 3201.36 Premium High Strength Film Resin
ExxonMobil LD 6821.LC Low Density Polyethylene Resin
ExxonMobil LLDPE LL 6201RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade)

PEXB200 / 37505

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.