MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Impact Grade, Filled

Material Notes: Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. Typical applications include circuit breakers, small motor bases and housings, appliance panels, terminal blocks, barrier strips, etc.

Durez 22257 is fungus resistant per Mil-I-631D and Mil-810 A/E-2572

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ASTM D792
Apparent Bulk Density 0.570 g/cc0.0206 lb/in³ASTM D1895
Water Absorption 0.60 %0.60 %ASTM D570
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 55.0 MPa7980 psiASTM D638
Tensile Modulus 7.60 GPa1100 ksiASTM D638
Flexural Strength 69.0 MPa10000 psi
Compressive Strength 193 MPa28000 psiASTM D695
Shear Strength 76.0 MPa11000 psias molded
Izod Impact, Notched 0.240 J/cm0.450 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM D257
Dielectric Constant 5.5
@Frequency 1e+6 Hz
5.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 7.90 kV/mm201 kV/inStep by step; ASTM D149
 8.90 kV/mm226 kV/inShort Time; ASTM D149
Dissipation Factor 0.080
@Frequency 1e+6 Hz
0.080
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 42.2 µm/m-°C
@Temperature 23.0 - 60.0 °C
23.4 µin/in-°F
@Temperature 73.4 - 140 °F
Specific Heat Capacity 1.42 J/g-°C0.339 BTU/lb-°F
Thermal Conductivity 0.402 W/m-K2.79 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C302 °FUL temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 149 °C300 °FASTM D648
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade
Overview of materials for Epoxy Molding Compound

P90X20 / 21137

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.