MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Aptek 2209-A/B Clear, non-yellowing urethane adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: APTEK 2209-A/B is a water clear, thixotropic, two component, electrically insulating, urethane adhesive designed for bonding various substrates. APTEK 2209-A/B is effective for bonding plastics and in particular displays excellent adhesion to GE LEXAN (polycarbonate) without cracking or crazing the substrate.

Excellent U.V. and weathering resistance for outdoor application. Very good clarity for see-through applications like back-lit signs/displays. Convenient 1:1 PBW or PBV mix ratio for easy handling. Fast set version available upon request. Low viscosity, castable version available upon request.

APTEK 220-A is a clear polyol resin. APTEK 2209B is a clear organic isocyanate.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³A Component; ASTM D1475
 1.14 g/cc0.0412 lb/in³B Component; ASTM D1475
Viscosity 76000 cP76000 cPB Component; ASTM D1824
 92000 cP92000 cPA Component; ASTM D1824
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 6050 - 60Cured property; ASTM D2240
Adhesive Bond Strength 4.83 MPa700 psiCured property; Lap Shear failure in polycarbonate substrate; ASTM D1002
 8.27 MPa1200 psiAl-to-Al Lap Shear; Cured property; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 150 °C>= 302 °FA Component; ASTM D92
 >= 150 °C>= 302 °FB Component; ASTM D92
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 °C212 °FCure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Encapsulant, Unreinforced
Aptek UVISTAKE 7206 UV Curing, Urethane staking compound
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
Overview of materials for Epoxy, High Temperature
Overview of materials for Cyanoacrylate Adhesive

PAPTEK06 / 24168

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.