MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPR 12222 Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Total Petrochemicals PPR 12222 is a high melt flow index, clarified random copolymer. Its high transparency makes it particularly suitable for the production of household articles and packaging. Its high fluidity accounts for significant cycle time reduction.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.902 g/cc0.902 g/ccISO 1183
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Melt Flow 60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
60 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8282ISO 2039-2
Flexural Modulus 1.10 GPa160 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point  67.0 °C
@Load 5.10 kg
153 °F
@Load 11.2 lb
50°C per hour; ISO 306
 130 °C
@Load 1.02 kg
266 °F
@Load 2.25 lb
50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding
BASF Ultramid® B3K PA6 (Dry)

PTOTAL834 / 130559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.